Số hiệu tiêu chuẩn
EN ISO 15609-5
Tên tiêu chuẩn
Specification and qualification of welding procedures for metallic materials - Welding procedure specification - Part 5: Resistance welding (ISO 15609-5:2011)
Ngày phát hành
2011-10-00
Tiêu chuẩn tương đương
DIN EN ISO 15609-5 (2012-03), IDT * BS EN ISO 15609-5 (2011-10-31), IDT * NF A89-052-5 (2011-12-01), IDT * ISO 15609-5 (2011-10), IDT * SN EN ISO 15609-5 (2012-01), IDT * OENORM EN ISO 15609-5 (2012-03-01), IDT * PN-EN ISO 15609-5 (2012-02-23), IDT * SS-EN ISO 15609-5 (2011-10-24), IDT * UNE-EN ISO 15609-5 (2012-06-20), IDT * UNI EN ISO 15609-5:2012 (2012-02-09), IDT * STN EN ISO 15609-5 (2012-04-01), IDT * CSN EN ISO 15609-5 (2012-05-01), IDT * DS/EN ISO 15609-5 (2011-11-25), IDT * NEN-EN-ISO 15609-5:2011 en (2011-10-01), IDT * SFS-EN ISO 15609-5 (2012-03-23), IDT * SFS-EN ISO 15609-5:en (2012-11-16), IDT
Tiêu chuẩn liên quan
ISO 4063 (2009-08) *
ISO 17677-1 (2009-07) * ISO 669 (2000-04) * ISO 5183-1 (1998-09) * ISO 5183-2 (2000-12) * ISO 5184 (1979-07) * ISO 5821 (2009-02) * ISO 5827 (1983-12) * ISO 8205-1 (2002-08) * ISO 8205-2 (2002-08) * ISO 8430-1 (1988-12) * ISO 8430-2 (1988-12) * ISO 8430-3 (1988-12) * ISO 8430-3 Technical Corrigendum 1 (1990-10) * ISO 15607 (2003-12) * ISO 15614-12 (2004-08) * ISO 15614-13 (2005-02)
Từ khóa
Approval * Blank forms * Electron-beam welding * Flash welding * Fusion welding * Materials * Metal welding * Metallic * Metallic materials * Metals * Pressure butt welding * Projection welding * Resistance welding * Roller seam welding * Specification (approval) * Spot welding * Suitability * Testing conditions * Training * Welded joints * Welding * Welding engineering * Welding procedure specification * Welding processes * Welds * Legalization * Acceptance