Số hiệu tiêu chuẩn
prEN ISO 15609-5
Tên tiêu chuẩn
Specification and qualification of welding procedures for metallic materials - Welding procedure specification - Part 5: Resistance welding (ISO/DIS 15609-1:2010)
Ngày phát hành
2010-06-00
Tiêu chuẩn tương đương
DIN EN ISO 15609-5 (2010-06), IDT * A89-052-5PR, IDT * ISO/DIS 15609-5 (2010-06), IDT * OENORM EN ISO 15609-5 (2010-07-15), IDT
Từ khóa
Approval * Blank forms * Electron-beam welding * Flash welding * Fusion welding * Materials * Metal welding * Metallic * Metallic materials * Metals * Pressure butt welding * Projection welding * Resistance welding * Roller seam welding * Specification (approval) * Spot welding * Suitability * Testing conditions * Welded joints * Welding * Welding engineering * Welding procedure specification * Welding processes * Welds * Legalization * Acceptance