Số hiệu tiêu chuẩn
ISO 15614-2
Tên tiêu chuẩn
Specification and qualification of welding procedures for metallic materials - Welding procedure test - Part 2: Arc welding of aluminium and its alloys
Ngày phát hành
2005-05-00
Tiêu chuẩn tương đương
DIN EN ISO 15614-2 (2005-07), IDT * BS EN ISO 15614-2 (2005-04-26), IDT * GB/T 19869.2 (2012), MOD * EN ISO 15614-2 (2005-04), IDT * NF A89-057-2 (2005-12-01), IDT * SN EN ISO 15614-2 (2005-08), IDT * OENORM EN ISO 15614-2 (2005-07-01), IDT * PN-EN ISO 15614-2 (2005-07-15), IDT * PN-EN ISO 15614-2 (2008-04-18), IDT * UNE-EN ISO 15614-2 (2006-03-01), IDT * GOST R ISO 15614-2 (2009), IDT * TS EN ISO 15614-2 (2007-03-27), IDT * UNI EN ISO 15614-2:2006 (2006-02-09), IDT * STN EN ISO 15614-2 (2005-11-01), IDT * CSN EN ISO 15614-2 (2006-01-01), IDT * DS/EN ISO 15614-2 (2005-06-27), IDT * NEN-EN-ISO 15614-2:2005 en (2005-06-01), IDT * NEN-EN-ISO 15614-2:2005 nl (2005-06-01), IDT * SANS 15614-2:2007 (2007-04-26), IDT
Thay thế cho
ISO 9956-4 (1995-09) * ISO 9956-4 AMD 1 (1998-11) * ISO/FDIS 15614-2 (2004-01)
Lịch sử ban hành
ISO 15614-2 (2005-05) * ISO/FDIS 15614-2 (2004-01) * ISO/DIS 15614-2 (2000-11) * ISO 9956-4 AMD 1 (1998-11) * ISO 9956-4 FDAM 1 (1998-07) * ISO 9956-4 DAM 1 (1996-05) * ISO 9956-4 (1995-09) * ISO/DIS 9956-4 (1992-10)
Từ khóa
Aluminium * Aluminium alloys * Approval * Approval tests * Arc welding * Cast materials * Definitions * Destructive testing * Fusion welding * Malleable materials * Materials * Metal welding * Metallic materials * Non-destructive testing * Specification (approval) * Test specimens * Testing * Training * Welding * Welding engineering * Welding procedure specification * Welding processes * Wrought alloys * Legalization * Acceptance