Số hiệu tiêu chuẩn
prEN ISO 15614-4
Tên tiêu chuẩn
Specification and qualification of welding procedures for metallic materials - Welding procedure test - Part 4: Finishing welding of aluminium castings (ISO/DIS 15614-4:2003)
Ngày phát hành
2003-07-00
Tiêu chuẩn tương đương
DIN EN ISO 15614-4 (2003-08), IDT * A89-057-4PR, IDT * ISO/DIS 15614-4 (2003-07), IDT
Từ khóa
Alloys * Aluminium * Aluminium casting * Aluminium wrought alloys * Approval * Approval tests * Arc welding * Building sites * Definitions * Fusion welding * Joint welding * Materials * Metal welding * Metallic materials * Metals * Production welding * Quality * Quality assurance * Specification (approval) * Suitability * Testing * Titanium * Titanium alloys * Titanium-containing alloys * Verification * Welding * Welding engineering * Welding filler metals * Welding procedure specification * Welding processes * Welding work * Zirconium * Zirconium-containing alloys * Legalization * Acceptance