Số hiệu tiêu chuẩn
NF A89-057-13*NF EN ISO 15614-13
Tên tiêu chuẩn
Specification and qualification of welding procedures for metallic materials - Welding procedure test - Part 13 : upset resistance butt and flash welding
Ngày phát hành
2012-08-01
Tiêu chuẩn tương đương
EN ISO 15614-13:2012,IDT * ISO 15614-13:2012,IDT
Tiêu chuẩn liên quan
ISO 4063 * ISO 4136 * ISO 5173 * ISO 6520-2 * ISO 6892-1 * ISO 9015-1 * ISO 9015-2 * ISO 11666 * ISO 14271 * ISO 14732 * ISO 15607 * ISO/TR 15608 * ISO 15609-5 * ISO 15620 * ISO 17637 * ISO 17638 * ISO 17639 * ISO 17640 * ISO 17643 * ISO 20482 * ISO 23277 * ISO 23278 * ISO 23279
Thay thế cho
NF EN ISO 15614-13:200506 (A89-057-13)
Từ khóa
Weldings * Approval * Non-destructive testing * Inspection * Resistance welding * Testing conditions * Qualifications * Welding * Welded joints * Metals * Trials * Legalization * Acceptance * Welding on * Training * Butt joints * Testing