ISO 11463

Corrosion of metals and alloys - Evaluation of pitting corrosion

Số trang: 10
Ngày phát hành: 1995-12-00

Liên hệ
Gives guidance on the selection of procedures that can be used in the identification and examination of pits and in the evaluation of pitting corrosion.
Số hiệu tiêu chuẩn
ISO 11463
Tên tiêu chuẩn
Corrosion of metals and alloys - Evaluation of pitting corrosion
Ngày phát hành
1995-12-00
Trạng thái
Có hiệu lực
Tiêu chuẩn tương đương
DIN EN ISO 11463 (2008-08), IDT * DIN EN ISO 11463 (2007-11), IDT * BS EN ISO 11463 (1996-09-15), IDT * GB/T 18590 (2001), IDT * EN ISO 11463 (2008-04), IDT * prEN ISO 11463 (2007-09), IDT * NF A05-323 (2002-06-01), IDT * NF A05-323 (2008-08-01), IDT * A05-323PR, IDT * SN EN ISO 11463 (2008-07), IDT * OENORM EN ISO 11463 (2008-07-01), IDT * OENORM EN ISO 11463 (2007-11-01), IDT * PN-EN ISO 11463 (2008-07-11), IDT * PN-EN ISO 11463 (2010-03-15), IDT * SS-EN ISO 11463 (2008-04-21), IDT * SS-ISO 11463 (1998-11-20), IDT * UNE-EN ISO 11463 (2009-09-09), IDT * TS EN ISO 11463 (2000-11-23), IDT * UNI EN ISO 11463:2008 (2008-09-18), IDT * STN EN ISO 11463 (2008-08-01), IDT * CSN ISO 11463 (1997-11-01), IDT * DS/EN ISO 11463 (2008-07-11), IDT * NEN-EN-ISO 11463:2008 en (2008-05-01), IDT
Tiêu chuẩn liên quan
ISO 8407 (1991-07)
Corrosion of metals and alloys; removal of corrosion products from corrosion test specimens
Số hiệu tiêu chuẩn ISO 8407
Ngày phát hành 1991-07-00
Mục phân loại 77.060. Ăn mòn kim loại
Trạng thái Có hiệu lực
Thay thế cho
ISO/DIS 11463 (1993-05)
Thay thế bằng
Lịch sử ban hành
ISO 11463 (1995-12)
Corrosion of metals and alloys - Evaluation of pitting corrosion
Số hiệu tiêu chuẩn ISO 11463
Ngày phát hành 1995-12-00
Mục phân loại 77.060. Ăn mòn kim loại
Trạng thái Có hiệu lực
* ISO/DIS 11463 (1993-05)
Từ khóa
Alloys * Corrosion * Corrosion resistance * Corrosion tests * Evaluations * Materials testing * Metals * Pitting * Pitting corrosion * Testing
Mục phân loại
Số trang
10