Số hiệu tiêu chuẩn
ISO 7539-1
Tên tiêu chuẩn
Corrosion of metals and alloys - Stress corrosion testing - Part 1: General guidance on testing procedures
Ngày phát hành
1987-08-00
Tiêu chuẩn tương đương
DIN EN ISO 7539-1 (1995-08), IDT * BS EN ISO 7539-1 (1988-07-29), IDT * GB/T 15970.1 (1995), IDT * EN ISO 7539-1 (1995-05), IDT * prEN ISO 7539-1 (1995-01), IDT * NF A05-501-1 (1991-12-01), IDT * NF A05-501-1 (1995-10-01), IDT * SN EN ISO 7539-1 (1995), IDT * OENORM EN ISO 7539-1 (1995-08-01), IDT * OENORM ISO 7539-1 (1994-04-01), IDT * PN-EN ISO 7539-1 (2000-02-24), IDT * SS-EN ISO 7539-1 (1995-10-13), IDT * SS-ISO 7539-1 (1993-08-31), IDT * UNE-EN ISO 7539-1 (1996-09-23), IDT * GOST 9.901.1 (1989), IDT * STN EN ISO 7539-1 (2001-10-01), IDT * CSN 03 8172-1 (1991-06-01), IDT * DS/EN ISO 7539-1 (1995-09-15), IDT * NEN-EN-ISO 7539-1:1995 en (1995-06-01), IDT
Thay thế bằng
ISO 7539-1 (2012-12)
Từ khóa
Alloys * Corrosion * Corrosion tests * Definitions * Materials testing * Metals * Stress corrosion * Tension crack corrosion * Testing