Specifies a test, using an ammoniacal atmosphere, for the detection of applied or residual stresses which can cause failure of the material in service or storage through stress corrosion cracking. The severity of the method can be regulated by changing the pH value. In an informative annex, recommendations are given for the choice of pH-values.
Số hiệu tiêu chuẩn
ISO 6957
Tên tiêu chuẩn
Copper alloys; ammonia test for stress corrosion resistance
Ngày phát hành
1988-10-00
Tiêu chuẩn tương đương
DIN 50916-1 (1976-08), MOD * JIS H 3300 (1997-09-20), MOD * OENORM ISO 6957 (1993-05-01), IDT * PN-ISO 6957 (1997-03-12), IDT * SS-ISO 6957 (1988-10-19), IDT * NEN-ISO 6957 (1988), IDT * NEN-ISO 6957:1988 en (1988-12-01), IDT
Từ khóa
Copper * Copper alloys * Corrosion resistance * Corrosion tests * Determination * Stress corrosion * Testing * Tests * Products