Số hiệu tiêu chuẩn
EN ISO 15614-11
Tên tiêu chuẩn
Specification and qualification of welding procedures for metallic materials - Welding procedure test - Part 11: Electron and laser beam welding (ISO 15614-11:2002)
Ngày phát hành
2002-03-00
Tiêu chuẩn tương đương
DIN EN ISO 15614-11 (2002-10), IDT * BS EN ISO 15614-11 (2002-03-28), IDT * NF A89-057-11 (2002-05-01), IDT * ISO 15614-11 (2002-03), IDT * SN EN ISO 15614-11 (2002-03), IDT * OENORM EN ISO 15614-11 (2002-10-01), IDT * PN-EN ISO 15614-11 (2005-02-15), IDT * SS-EN ISO 15614-11 (2002-12-13), IDT * UNE-EN ISO 15614-11 (2002-10-22), IDT * TS EN ISO 15614-11 (2009-04-28), IDT * UNI EN ISO 15614-11:2003 (2003-06-01), IDT * STN EN ISO 15614-11 (2002-11-01), IDT * CSN EN ISO 15614-11 (2003-06-01), IDT * DS/EN ISO 15614-11 (2002-09-16), IDT * DS/EN ISO 15614-11 (2007-07-30), IDT * NEN-EN-ISO 15614-11:2002 en (2002-04-01), IDT * SFS-EN ISO 15614-11:en (2002-05-07), IDT
Từ khóa
Acceptance * Approval * Blank forms * Certification * Definitions * Destructive testing * Electric welding * Electron beams * Electron-beam welding * Forms (paper) * Inspection * Instructions * Laser beam welding * Laser beams * Materials * Metallic materials * Metals * Quality * Quality assurance * Quality requirements * Specification (approval) * Suitability * Testing * Verification * Welding * Welding engineering * Welding filler metals * Welding procedure specification * Welding processes * Welding work * Legalization