ASTM G 8

Standard Test Methods for Cathodic Disbonding of Pipeline Coatings

Số trang: 9
Ngày phát hành: 1996-00-00

Liên hệ
1.1 These test methods cover accelerated procedures for simultaneously determining comparative characteristics of insulating coating systems applied to steel pipe exterior for the purpose of preventing or mitigating corrosion that may occur in underground service where the pipe will be in contact with inland soils and may or may not receive cathodic protection. They are intended for use with samples of coated pipe taken from commercial production and are applicable to such samples when the coating is characterized by function as an electrical barrier. 1.2 This test method is intended for testing coatings submerged or immersed in the test solution at room temperature. When it is impractical to submerge or immerse the test specimen, Test Method G 95 may be considered where the test cell is cemented to the surface of the coated pipe specimen. If higher temperatures are required, see Test Method G 42. If a specific test method is required with no options, see Test Method G 80. 1.3 The values stated in SI units to 3 significant decimals are to be regarded as the standard. The values given in parentheses are for information only. This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Số hiệu tiêu chuẩn
ASTM G 8
Tên tiêu chuẩn
Standard Test Methods for Cathodic Disbonding of Pipeline Coatings
Ngày phát hành
1996-00-00
Trạng thái
Có hiệu lực
Tiêu chuẩn tương đương
Tiêu chuẩn liên quan
Thay thế cho
ASTM G 8 (1990)
Test Methods for Cathodic Disbonding of Pipeline Coatings
Số hiệu tiêu chuẩn ASTM G 8
Ngày phát hành 1990-00-00
Mục phân loại 23.040.99. Các phụ tùng đường ống khác
Trạng thái Có hiệu lực
Thay thế bằng
Lịch sử ban hành
ASTM G 8 (1996)
Standard Test Methods for Cathodic Disbonding of Pipeline Coatings
Số hiệu tiêu chuẩn ASTM G 8
Ngày phát hành 1996-00-00
Mục phân loại 23.040.99. Các phụ tùng đường ống khác
Trạng thái Có hiệu lực
* ASTM G 8 (1990)
Test Methods for Cathodic Disbonding of Pipeline Coatings
Số hiệu tiêu chuẩn ASTM G 8
Ngày phát hành 1990-00-00
Mục phân loại 23.040.99. Các phụ tùng đường ống khác
Trạng thái Có hiệu lực
* ASTM G 8 (1985)
Test Methods for Cathodic Disbonding of Pipeline Coatings
Số hiệu tiêu chuẩn ASTM G 8
Ngày phát hành 1985-00-00
Mục phân loại 25.220.40. Lớp mạ kim loại
Trạng thái Có hiệu lực
* ASTM G 8 (1979)
Test Methods for Cathodic Disbonding of Pipeline Coatings
Số hiệu tiêu chuẩn ASTM G 8
Ngày phát hành 1979-00-00
Mục phân loại 25.220.40. Lớp mạ kim loại
Trạng thái Có hiệu lực
Từ khóa
Adhesiveness * Coatings * Electrical * Materials * Non-metals * Painting * Paints * Permanency * Pipelines * Testing * Durability
Số trang
9